The Domite®
Standard
Uncompromising abrasion resistance for extreme industrial environments. Engineered to survive where standard steel fails.
9.5x
Increased Wear Life
Metallurgical Data Correction
| Material Designation | Hardness (BHN) | Hardness (Rc) | Yield (MPa) | Tensile (MPa) |
|---|---|---|---|---|
| Standard Steel (ASTM A36) | 120 - 160 | -- | 250 MPa (36 ksi) | 400 MPa (58 ksi) |
| Domite® (Chrome White Iron - Grade HC 25) | 700 BHN | 63 Rc | 750 MPa | 900 MPa |
| Hardox 450 | 450 BHN | 45 Rc | 1200 MPa | 1400 MPa |
Standard Steel
vs. Domite®
Visualizing the 9.5x wear life differential in high-velocity impact testing. Standard A36 steel shows significant plastic deformation and surface loss under identical stress parameters.
01 / MICROSTRUCTURE
Carbide Density
M7C3 chromium carbides provide the primary wear protection, embedded in an austenitic matrix for maximum impact toughness.
02 / BONDING
Metallurgical Weld
Vacuum furnace brazing ensures a continuous metallurgical bond between the wear surface and the mild steel backing plate.
03 / GEOMETRY
Custom Casting
Our precision casting process allows for complex shapes that reduce mechanical stress points in high-load applications.